1. Kiln firing: Kiln firing is a very time-consuming step, the time process is about one day and night, and the temperature is around 1300°C. First build the kiln door, ignite the kiln, the fuel is pine wood, guide the piling technology, measure the fire, master the kiln temperature change, and decide the ceasefire time.
2. Color glaze: The color on the glaze, such as multicolored, pastel, etc., is to describe patterns and fill colors on the glazed surface of the fired porcelain, and then bake it in a red furnace at a low temperature of about 700-800 °C. In addition, before firing the kiln, painting on the green body, such as blue and white, underglaze red, etc., is called underglaze red, which is characterized by the fact that the color is under high temperature glaze and will never fade.
3. Glazing: In the process of glazing, the ordinary round mouth is dipped or glazed, and the cutter or large round ware is blown with glaze (the method is to cover the bamboo tube with spun yarn, and then blow it with the mouth after dipping in the glaze. Repeat this many times. glaze layer of uniform thickness).